Sintered NdFeB Magnet
Sintered NdFeB Magnet Corporalis Proprietatibus | ||||||||
Gradus | Remanentia | Rev. Temp.- Coeff. Domini Br | Coactio vis | Coactio intrinseca vis | Rev. Temp.- Coeff. Domini Hcj | Maximilianus. Energy Product | Maximilianus. Operating Temperature | Densitas |
Br (KGs) | Hcb (TU) | Hcj (TU) | (BH) max. (MGOe) | g/cm³ | ||||
N35 | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥12 | -0.58~-0.78 | 33-36 | 80℃ | 7.6 |
N38 | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥12 | -0.58~-0.78 | 36-39 | 80℃ | 7.6 |
N40 | 12.5-12.8 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 38-41 | 80℃ | 7.6 |
N42 | 12.8-13.2 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 40-43 | 80℃ | 7.6 |
N45 | 13.2-13.8 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 43-46 | 80℃ | 7.6 |
N48 | 13.8-14.2 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 46-49 | 80℃ | 7.6 |
N50 | 14.0-14.5 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 48-51 | 80℃ | 7.6 |
N52 | 14.3-14.8 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 50-53 | 80℃ | 7.6 |
N33M | 11.3-11.7 | -0.11~-0.12 | ≥10.5 | ≥14 | -0.58~-0.72 | 31-33 | 100℃ | 7.6 |
N35M | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥14 | -0.58~-0.72 | 33-36 | 100℃ | 7.6 |
N38M | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥14 | -0.58~-0.72 | 36-39 | 100℃ | 7.6 |
N40M | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥14 | -0.58~-0.72 | 38-41 | 100℃ | 7.6 |
N42M | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥14 | -0.58~-0.72 | 40-43 | 100℃ | 7.6 |
N45M | 13.2-13.8 | -0.11~-0.12 | ≥12.5 | ≥14 | -0.58~-0.72 | 43-46 | 100℃ | 7.6 |
N48M | 13.6-14.3 | -0.11~-0.12 | ≥12.9 | ≥14 | -0.58~-0.72 | 46-49 | 100℃ | 7.6 |
N50M | 14.0-14.5 | -0.11~-0.12 | ≥13.0 | ≥14 | -0.58~-0.72 | 48-51 | 100℃ | 7.6 |
N35H | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥17 | -0.58~-0.70 | 33-36 | 120℃ | 7.6 |
N38H | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥17 | -0.58~-0.70 | 36-39 | 120℃ | 7.6 |
N40H | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥17 | -0.58~-0.70 | 38-41 | 120℃ | 7.6 |
N42H | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥17 | -0.58~-0.70 | 40-43 | 120℃ | 7.6 |
N45H | 13.2-13.6 | -0.11~-0.12 | ≥12.1 | ≥17 | -0.58~-0.70 | 43-46 | 120℃ | 7.6 |
N48H | 13.7-14.3 | -0.11~-0.12 | ≥12.5 | ≥17 | -0.58~-0.70 | 46-49 | 120℃ | 7.6 |
N35SH | 11.7-12.2 | -0.11~-0.12 | ≥11.0 | ≥20 | -0.56~-0.70 | 33-36 | 150℃ | 7.6 |
N38SH | 12.2-12.5 | -0.11~-0.12 | ≥11.4 | ≥20 | -0.56~-0.70 | 36-39 | 150℃ | 7.6 |
N40SH | 12.5-12.8 | -0.11~-0.12 | ≥11.8 | ≥20 | -0.56~-0.70 | 38-41 | 150℃ | 7.6 |
N42SH | 12.8-13.2 | -0.11~-0.12 | ≥12.4 | ≥20 | -0.56~-0.70 | 40-43 | 150℃ | 7.6 |
N45SH | 13.2-13.8 | -0.11~-0.12 | ≥12.6 | ≥20 | -0.56~-0.70 | 43-46 | 150℃ | 7.6 |
N28UH | 10.2-10.8 | -0.11~-0.12 | ≥9.6 | ≥25 | -0.52~-0.70 | 26-29 | 180℃ | 7.6 |
N30UH | 10.8-11.3 | -0.11~-0.12 | ≥10.2 | ≥25 | -0.52~-0.70 | 28-31 | 180℃ | 7.6 |
N33UH | 11.3-11.7 | -0.11~-0.12 | ≥10.7 | ≥25 | -0.52~-0.70 | 31-34 | 180℃ | 7.6 |
N35UH | 11.8-12.2 | -0.11~-0.12 | ≥10.8 | ≥25 | -0.52~-0.70 | 33-36 | 180℃ | 7.6 |
N38UH | 12.2-12.5 | -0.11~-0.12 | ≥11.0 | ≥25 | -0.52~-0.70 | 36-39 | 180℃ | 7.6 |
N40UH | 12.5-12.8 | -0.11~-0.12 | ≥11.3 | ≥25 | -0.52~-0.70 | 38-41 | 180℃ | 7.6 |
N28EH | 10.4-10.9 | -0.105~-0.120 | ≥9.8 | ≥30 | -0.48~-0.70 | 26-29 | 200℃ | 7.6 |
N30EH | 10.8-11.3 | -0.105~-0.120 | ≥10.2 | ≥30 | -0.48~-0.70 | 28-31 | 200℃ | 7.6 |
N33EH | 11.3-11.7 | -0.105~-0.120 | ≥10.5 | ≥30 | -0.48~-0.70 | 31-34 | 200℃ | 7.6 |
N35EH | 11.7-12.2 | -0.105~-0.120 | ≥11.0 | ≥30 | -0.48~-0.70 | 33-36 | 200℃ | 7.6 |
N38EH | 12.2-12.5 | -0.105~-0.120 | ≥11.3 | ≥30 | -0.48~-0.70 | 36-39 | 200℃ | 7.6 |
N28AH | 10.4-10.9 | -0.105~-0.120 | ≥9.9 | ≥33 | -0.45~-0.70 | 26-29 | 230℃ | 7.6 |
N30AH | 10.8-11.3 | -0.105~-0.120 | ≥10.3 | ≥33 | -0.45~-0.70 | 28-31 | 230℃ | 7.6 |
N33AH | 11.3-11.7 | -0.105~-0.120 | ≥10.6 | ≥33 | -0.45~-0.70 | 31-34 | 230℃ | 7.6 |
Nota: · Sub operando temperatus 20℃±2℃, supra parametri magnetici et physicas proprietates probantur, cum inevitabili detrimento vis magneticae non plus quam 5%.· Maximae operationis temperaturae magnetis mutabilis est propter rationem longitudinis et diametri et ambitus factorum. . |
Commodum:
Horum magnetum proprietates longe praestantiores sunt maioribus traditis et nunc maxime in applicatione sunt potentissimi. Summus eorum
coactivam et altam remanentiam permittere novum consilium et facultatem augendi campum magneticum applicationis ubi spatium limitatum est
vel ubi fortis campus magneticus requiritur.
Magnetes ndFeB valde corrosioni obnoxii sunt. Ergo superficies membrana tutela require. Usus magnetis NdFeB conditionatus
temperatura in amplis cursus ab 80ºC ad 230ºC. Atque etiam in temperie infra 0℃ operatur.
Applicatio:
Magnetes Neodymium magneticae variae genera lentium magneticarum ad positionem, deflexionem particularum accusatorum in electronicis systematibus confregit;
stillat, sensorem, systema magneticum in rotor et micro motoribus, et scientia, medicina (tomographia, NMR spectrometris), etc.
Hodie, magnetes NdFeB in toto orbe terrarum magnae quantitates adhibentur. Huius materialis explicatio nondum perfecta est; remanentia
et coercitiva agri vires continue augentur. Magna vis magnetum NdFeB significat motores et sensories aedificari posse
semper minor — et hoc significat incrementum in effectu efficientiae. Emendationes permanentes sinunt hanc materiam interesting ut conti-
nually in novis locis.
Omnes valores statuti determinati sunt utentes exemplaria regulae secundum IEC 60404-5. Specificationes sequentes serve ad valores referendi et
differant. Ad maiorem informationem quaeso contact applicationem machinarum nostrorum.